First attempt at Pate De Verre

 


Todays demo was on Pate De Verre (Paste of glass)  and I thought I would have a little go myself!

What you need for this is a plaster mould, a teaspoon, some frit (fine or powder is better) and a mix of 50/50 Glasstac and water.

You mix up the frit and glasstac mix to a thick gritty paste, almost like sugar topping.



Then you take the teaspoon and press the paste into the mould, compacting it as much as possible.

 


I also added a little blue glass mix at this stage too to make it a little more interesting.

Once you are happy with the thickness of the glass paste, you pack the remainder of the mould with a pre-fired plaster to stop the glass collapsing during firing.

Then off to the kiln to be fired at 765 degrees for an hour.


When it is cold you shake the powdered plaster out – wearing a mask so you don’t breath in any nasty particles.


Then you can carefully chip away and break the mould off to reveal your glass work underneath.


Not bad for my first go.  Not sure it will be a favourite technique as it’s not hugely tactile to tough and hold, but I enjoyed trying the process.




Thursday, 10 March 2022

Experimenting with marbles

  have melted marbles in the kiln quite a few times over the years, to make pin badges, tie-pins and other stuff.

But this time I wanted to see if I could fuse some to window glass.

The hardest job is getting all the little buggers to stay in the right place, as once you knock one it is like a domino effect and they roll about all over the place.


After a bit of swearing, and much more time than this deserved, I seemed to have them all laid out nicely in the kiln.



I placed a few on top of a small square of window glass – these too had the tendency to roll about, but we got there in the end.

The following morning I opened the kiln with anticipation, wondering if I would find a heap of melted marbles all in one corner of the kiln, but luckily they had stayed put and fused down nicely.


And the best bit was…. My experiment had worked too!


With no incompatibility cracks either would you believe?

 


Result!

Monday, 31 January 2022

Lost Wax Casting - my own hand!

 


We were learning how to use silicon casting material today to take a nice detailed cast of items – which can then be made into wax and finally glass.

 So, I thought I would do my hand, complete with jewellery to see how much detail I could get.

 So I plunged my hand into the bucket and waited a little while for it to set – then after a slight wriggle or two, I was free!

The next step was to pour melted wax into the mould, and wait for that to harden.

Once the wax was set I could break away the silicon mould – I then set the waxy hand on a lump of clay to form a base.


Plaster Recipe for refractory mould:  (to be measured up as required)

·       1lb plaster powder

·       1lb molochite powder

·       1 pint water

Now it was time to cover the hand in the plaster mix.  Adding layers at a time to ensure all the parts were covered.


When the mould was dry, it was time to scrape out the clay and melt out the wax. 

This was done over a steamer, allowing the wax to drip into a tray which meant it could be reused.

Once the wax was out I have to fill the mould with water to measure how much glass I would need  (2.5 x the amount of water)

The mould was then put into the drying cupboard.

Once dry, I filled a terracotta plant pot with the correct amount of glass and they went into the kiln.

The mould was positioned with a table above made from kiln props, on this sat a plant pot with my measured amount of glass in it.  Once the glass melted it dripped through the hole in the plant pot down into the mould.

I used some scrap glass from the HotShop to make this as I fancied a little colour.


Now it was time to very carefully chip away the mould, making sure not to damage the glass inside.


Dah da!    A lovely glass hand …. minus a little pinkie  😊

 It was at this point that I realised I had not added any cocktail sticks to help air and glass flow – lesson learnt.

The silicon mould doesn’t last long and is not really reusable over time, but I managed to get another wax cast from it.

This piece didn’t need any coldworking at all, I purposely underestimated the glass amount needed so I didn’t have much (or any) overspill, and it all came out quite smooth.




Sunday, 21 November 2021

Refractory Mould – Nuts & Bolts

The first thing I had to do for this project was to create textures in a block of clay.

 


I found some screws and bolts and a wingnut and pressed them into a squared off block of clay.  I thought they would make some interesting textures – bold and easy to see what they were.

Next I built a box around my clay using Cottle boards and clamps.   Around the bottom of the boards I added a little clay so none of the plaster mix would leak out.

 


Plaster Recipe for refractory mould:  (to be measured up as required)

·       1lb plaster powder

·       1lb molochite powder

1 pint water

Once the plaster mould was dry, I could gently remove all of the clay.

I washed off all the tiny remaining bits with a toothbrush and water.

The next job was to fill the mould with water and measure it.

 

It’s important to do this BEFORE the mould is put in to the drying cupboard as doing it afterwards would allow the mould to absorb more water, causing issues in the kiln.

I scratched on the side the amount of water needed to fill it – 260ml.



The mould then went into the drying cupboard for about a week to make sure it was thouroughly dried. 

Now it was time to work out how much glass I needed.

A = the amount of water that fills the mould

A x 2.5 = the weight of glass needed to fill the cavity.

So this one was 260 x 2.5 = 650 grams

I weighed this amount out and positioned it into the mould.

Finally the mould and glass went into the kiln so the glass could melt into all of the crevices.


Once out of the kiln I could gently break away and discard the mould material, leaving the slab of glass.

  

I have put a little too much glass in this mould, hence the overflow, but it will be interesting to cold work it to bring it back to shape.


I used the flat bed grinder in the coldshop to grind all of the excess glass off this piece. I used 120 grit at first, moving on to 320 grit once I had the shape I liked.

I actually had to stop at that point as I could see some stress in the corner of the piece which I suspect would have chipped the corner off if I had continued.

Still,  I am rather pleased with the result, and cannot wait to have another go.



Friday, 26 February 2021

My sustainability project.

  I have finished my uni piece for my 'Sustainability' assignment.

Due to the fact the working with glass isn't one of the most sustainable art forms, I decided to create a piece that might draw attention to the plight of the planet instead.  

I also decided that I would not purchase anything to create this piece, but concentrated on working with things I already had.

In my head I wanted to make a clock, to draw attention to the fact that we have limited time left to help the planet.

I had a box of mini wine bottles that I scrubbed and dried, then popped in the kiln to melt down flat.

My kiln is quite an energy efficient one, as it's not soo big, but I did need to do a couple of firings to complete my piece.

Once they were flat I messed about for a bit trying to decide on a formation. Ideally I would have liked to use all twelve bottles, but this was going to make the clock too heavy to hang.  In the end I decided on a formation of eight bottles, leaving some to use in another project at a later date.

I cut the numbers out of old copper sheet that I had rescued from a fire pit.


Once that was all nicely fused I was just going to fit a clock part, when I came across a clock kit in my stash that had an interesting wooden ring. Immediately I thought this would be excellent as a 'warning' ring if painted red.  Warning road signs are usually red rings.  

Because there was also another piece of round wood in the kit, I could sandwich the glass in-between the pieces with glass glue and bolts - therefore making it a much sturdier piece to hang on the wall.


As I now had a red warning ring I felt like I needed a warning statement to go on it.  My daughter helped me out with that - I wanted both the words 'Time' and 'Waste' within it.  She she wrote... "Don't call time on the Earth, reuse, don't waste". That worked really well so I wrote it on.

I was VERY unhappy with this as my handwriting is appallingly bad.  So it was back to the drawing board for that.

After a quick repaint, I dug out my vinyl cutting machine and I had some scraps of black vinyl left that had come from my old shop many years ago.  I cut out the words by machine this time and it looked so much better.  Using the vinyl was something I wanted to avoid if possible, due to it being plastic.  If it wasn't lockdown and I could have found someone with nice handwriting I would have definitely done it that way instead.


Now it was time to put it all together and add the clock mechanism.


And my piece was finished.  And it holds it's own weight well on the wall... and you can tell the time so it's functional too, as well as being a conversation starter,

I have enjoyed this project. I particularly like working with materials that might have otherwise gone in the bin.  Giving something a repurpose is something I try to do in other aspects of my life, like adapting clothing and sprucing up furniture.  So this assignment was right up my street.

Tuesday, 23 February 2021

Thanking the Kiln Gods.

  The Kiln Gods were good to me overnight, when I opened the lid of 'big blue' my faithful kiln I was so relieved to see a piece that had worked how I wanted it to.  Always a risky business using recycled glass.


It had slumped down pretty evenly and the numbers had worked.  Big thumbs up all round.

So, off I went to my craft shed to find a clock mechanism that I know I have somewhere as I save all sorts of stuff for 'just-in-case'.

Instead of just finding a mechanism, I actually found a clock kit that someone had gifted me a few years back... now my idea had evolved somewhat, I could use this piece to add something else to the design.


The kit consisted of a wooden clock base, along with a wooden ring and the clock part.

I decided that the ring needed to be bright red... like a warning ring, to warm people about time ticking away to save our planet.

So I painted it all red.



I am going to give it another couple of coats, then work out how to assemble it all!


Monday, 15 February 2021

Slumped Glass for my Metamorphosis project.

  I opened the kiln this morning to find some rather pleasing pieces of slumped glass.

They had all worked as I expected..... as one off pieces.





However, on putting them together (as I had originally planned) I found that one piece didn't work at all.... however, three pieces fit together so it was a great starting point.


I think it fits the brief - using two opposite words and showing the metamorphosis between,

I actually chose two sets of words to work opposite to each other. One was 'Clear to Opaque' and the other was 'Bud to Bloom'  So far it seems to work.


This piece (below) I shall put back into the kiln to re-fire. Although I have never had much success with re-firing work as it doesn't slump in the desired way.... glass has a habit of doing it's own thing sometimes.


So, I now have three pieces of my five needed for my metamorphosis assignment.  Just need to work on two more   :)